Original language | English (US) |
---|---|
Pages (from-to) | 55-60 |
Number of pages | 6 |
Journal | Scripta Metallurgica |
Volume | 15 |
Issue number | 1 |
DOIs | |
State | Published - Jan 1981 |
Analysis of stress corrosion crack-tip surface chemistries in 7075 type aluminum alloys
E. C. Pow, W. W. Gerberich, L. E. Toth
Research output: Contribution to journal › Article › peer-review
7
Scopus
citations