Dive into the research topics of 'High temperature nanoindentation of Cu–TiN nanolaminates'. Together they form a unique fingerprint.- Sort by
- Weight
- Alphabetically
Jeffrey M. Wheeler, Cayla Harvey, Nan Li, Amit Misra, Nathan A. Mara, Xavier Maeder, Johann Michler, Siddhartha Pathak
Research output: Contribution to journal › Article › peer-review