Nanoindentation probing of environmental effects on polymer coating properties

X. Xia, D. Roweniiorst, K. B. Yoder, L. E. Scriven, W. W. Gerberich

Research output: Contribution to journalConference articlepeer-review

Fingerprint

Dive into the research topics of 'Nanoindentation probing of environmental effects on polymer coating properties'. Together they form a unique fingerprint.

Engineering & Materials Science

Physics & Astronomy

Chemical Compounds